Physical characters | Unit | Properties |
SIC content | % | 95-88 |
Free Si | % | 5~12 |
Bulk density | g/cm3 | >3.01 |
Porosity | % | <0.1 |
Hardness | Kg/mm2 | 2400 |
Coefficient of bending strength at 20 degrees Celsius | Mpa | 260 |
Coefficient of bending strength at 1200 degrees Celsius | Mpa | 280 |
Modulus of elasticity at 20 Degrees Celsius |
Gpa | 330 |
Fracture toughness | Mpa*m1/2 | 3.3 |
Coefficient of thermal conductivity at 1200 degrees Celsius | W/m.k | 45 |
Coefficient of thermal expansion at 1200 degrees Celsius | 10-6mm/mmK | 4.5 |
Coefficient of heat radiation | <0.9 | |
Max. Working temperature | ºC | <1380 |
Note: Data of properties quoted are typical results from test pieces and therefore should be used only as a guidance |