Item | Main composition |
Diameter Range (mm) |
Density (g/cm3) |
Color | Vickers Hardness (kgf/mm2) |
Application Suggestion | |||||||
CS -26 | Al2O3 SiO2: |
0.5~20 | 2.6~2.8 | White | 700-800 | It's suitable for the stirred mill such as Metso's SMD and fine milling process of soft materials with low slurry density. | |||||||
CS-32 | Al2O3, SiO2 ZrO2 |
0.5~20 | 3.2~3.3 | White | 900-1000 | It's suitable for the stirred mill such as Metso's SMD and milling the hard minerals. | |||||||
CS- 36 | Al2O3 | 0.4~25 | 3.5~3.75 | White | 1300~1350 | It suitable for the Nano-size material grinding. | |||||||
CS- 40 | ZrO2 SiO2 |
0.4~5.0 | 4.0~4.2 | White | 1000~1050 | It's suitable for the high linear velocity conditions. Example, vertical and horizontal stirred mill, such as Outotec's HIGMill, Glencore's Isa mill. FLSmidth's VXP mill. It can grind the high density slurry of minerals. | |||||||
CS-52 | ZrO2 Al2O3 |
0.4~5.0 | 5.1-5.3 | White | 1350~1450 | It suitable for the hard materials's superfine mills with high speed (up to 14m/S) and high energy input. For example: Outotec's HIG mill. Flsmidth VXP. | |||||||
CS -60 | ZrO2 Y2O3 |
0.2~40 |
5.95~6.05 |
White | 1300~1400 |
|
|||||||
CS-62 | ZrO2:93~94% CeO2:6~7% |
0.6~4.0 | 6.1~6.2 | Yellow Or Brown |
1200~1250 |