| Item | Unit | Value |
| Ignition loss(700ºC) | % | 0.2 |
| AL2O3 | % | 0.45 |
| FSi,SiO2 | % | 13.04 |
| Fe2O3 | % | 0.33 |
| CaO | % | 0.058 |
| MgO | % | <0.01 |
| K2O | % | 0.03 |
| Na2O | % | 0.04 |
| TiO2 | % | <0.01 |
| SiC | % | 85 |
| Item | Unit | Value |
| Max working temperature | ºC | 1380 |
| Density | g/cm3 | ≥3.02 |
| Open porosity | % | <0.1 |
| Bending strength | Mpa | 250(20ºC) |
| Mpa | 280 (1200ºC) | |
| Modulus of elasticity | Gpa | 330(20ºC) |
| Gpa | 300(1200ºC) | |
| Thermal conductivity | W/m.K | 45(1200ºC) |
| Coefficient of thermal expansion | K¯¹x 10¯6 | 4.5 |
| Moh's hardness | Grade | 13 |